With the advantages of high efficiency, good effect, high precision, and easy automation integration, laser welding machines are widely used in various industries and play a pivotal role in industrial production and manufacturing. , mechanical meal gold, new energy, bathroom hardware and other industries have been fully utilized.

However, if any processing method does not master its principle and process, it will produce certain defects, and the laser welding machine is no exception. Only by better understanding these defects, how to avoid these defects, can the value of laser welding be better utilized, and products with beautiful appearance and high quality can be processed. The following QY Laser summarizes the solutions to some common welding defects for your reference!

_20220112112602

Cracks during welding

The cracks generated in laser continuous welding are mainly thermal cracks, such as crystallization cracks, liquefaction cracks, etc. The reason is mainly caused by the large shrinkage force of the weld before it is completely solidified, and measures such as wire filling and preheating can be reduced. or eliminate cracks.

Air holes appear during welding

Porosity is a defect that is easily generated in laser welding. The molten pool of laser welding is deep and narrow, and the cooling rate is fast. The gas generated in the liquid molten pool does not have enough time to escape, which easily leads to the formation of pores. However, laser welding cools quickly, and the pores generated are generally smaller than those of traditional fusion welding. Cleaning the surface of the workpiece before welding can reduce the tendency of porosity, and the direction of blowing will also affect the generation of porosity.

Undercut during welding

If the welding speed is too fast, the liquid metal at the back of the small hole pointing to the center of the weld will not have time to redistribute, and will solidify on both sides of the weld to form an undercut. If the joint assembly gap is too large, the molten metal of the caulking is reduced, and it is easy to produce undercuts. At the end of laser welding, if the energy drop time is too fast, the small hole is easy to collapse, resulting in local undercut. Controlling the matching of power and speed can well solve the generation of undercut. If the welding speed is slow, the molten pool is large and wide, the amount of molten metal increases, and the surface tension is difficult to maintain the heavier liquid metal, the center of the weld will sink, forming collapses and pits. At this time, it is necessary to appropriately reduce the energy density to avoid The molten pool collapses.